Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2950 cP @Temperature 25.0 °C |
2950 cP @Temperature 77.0 °F |
|
BASF Pluracol® 4850 Slabstock HR & Molded Graft Polyol Description: Pluracol® 4850 polyol is a primary hydroxyl-terminated graft polyether triol containing approximately 32% solids of copolymerized styrene and acrylonitrile, utilizing a LVI inhibitor p.. |