Material Notes:
Processed by anionic polymerization of caprolactam in the presence of a catalyst and activator. Uses include semi-finished products and containers (e.g. heating oil tanks).Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Dry as molded.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
Elongation at Break >= 50 %
>= 50 %
Elongation at Yield 20 %
20 %
Tensile Modulus 1.50 GPa
218 ksi
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm