Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ecoflex® F BX 7011 Biodegradable Plastic

Category Polymer , Film , Renewable/Recycled Polymer
Manufacturer BASF
Trade Name Ecoflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ecoflex® F BX 7011 Biodegradable Plastic.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film extrusion is a particular area where Ecoflex F shows well-balanced processing properties, and the resin can also be used in extrusion coating applications.
Physical Properties Metric English Comments
Density 1.25 - 1.27 g/cc
0.0452 - 0.0459 lb/in³
ISO 1183
Moisture Vapor Transmission 140 cc-mm/m²-24hr-atm
356 cc-mil/100 in²-24hr-atm
100% RH; ASTM Test
Oxygen Transmission Rate 1600 cc/m²/day
103 cc/100 in²/day
0% RH; ASTM Test
Melt Flow 2.7 - 4.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.7 - 4.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Yield, MD 560 %
560 %
ASTM Data
Film Elongation at Yield, TD 700 %
700 %
ASTM Data
Thermal Properties Metric English Comments
Melting Point 110 - 120 °C
230 - 248 °F
10 K/min
Optical Properties Metric English Comments
Transmission, Visible 82 %
82 %
Descriptive Properties Value Comments
Color Transparent
Commercial Status North America and Europe
Impact Modified No
Primary Processing Technique Blown Film
Users viewing this material also viewed the following: