Physical Properties Metric English Comments
Melt Flow 2.7 - 4.9 g/10 min
2.7 - 4.9 g/10 min
ISO 1133
BASF Ecoflex® 1200 F Blend Biodegradable Polyester
Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L..
Melt Flow 2.7 - 4.9 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.7 - 4.9 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
BASF Ecoflex® F BX 7011 Biodegradable Plastic
A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film e..
Melt Flow 2.7 - 4.9 g/10 min
2.7 - 4.9 g/10 min
ISO 1133
BASF Ecoflex® C1200 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E..