Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 140 cc-mm/m²-24hr-atm | 356 cc-mil/100 in²-24hr-atm | 100% RH; ASTM Test |
BASF Ecoflex® F BX 7011 Biodegradable Plastic A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film e.. |