Physical Properties Metric English Comments
Oxygen Transmission Rate 1600 cc/m²/day
103 cc/100 in²/day
0% RH; ASTM Test
BASF Ecoflex® F BX 7011 Biodegradable Plastic
A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film e..
Oxygen Transmission Rate 1600 cc/m²/day
103 cc/100 in²/day
DIN 53380
BASF Ecoflex® C1200 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E..