Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Mobil Centaur Moly 1

Category Fluid , Lubricant , Calcium Gellant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil Centaur Moly 1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil Centaur Moly is a premium quality grease formulated with advanced calcium sulfonate thickener technology. The calcium sulfonate thickener in the Mobil Centaur Moly  products represents a significant advance in grease formulation technology. Unlike conventional soap-base thickeners (i.e. lithium, aluminium, and calcium soaps), the calcium sulfonate thickener does much more than simply impart consistency. It imparts excellent corrosion and water-resistance properties to the grease and has inherent extreme-pressure protection properties that enhance load-carrying ability. Further, the EP properties derived from the calcium thickener also have inherently better thermal stability than those from conventional Sulphur/Phosphorus EP additives. Fortified with molybdenum disulphide to complement its robust extreme-pressure additive system, Mobil Centaur Moly  is particularly well suited to meet the demanding lubrication requirements of heavy-duty truck chassis, construction and mining equipment, and heavily load industrial bearings. Mobil Centaur Moly  also provides outstanding resistance against the effects of water washout, water spray-off and corrosion.Mobil Centaur Moly  products are highly recommended for heavily loaded applications or environments highly contaminated with water. Specific examples of such applications include: Heavy-duty trucks, including chassis, spring shackles, king pins, tie rods, u-joints, hinge and bucket pins and fifth wheels; Mining and construction equipment; Marine equipment; Highly loaded industrial bearings
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 320 cSt
320 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
ASTM D2596
Four Ball Wear 0.500 mm
0.0197 in
40 kg, 1200 rpm; ASTM D2266
Penetration 325
325
Worked, 25°C; ASTM D217
Timken Test 27200 g
60.0 lb
Thermal Properties Metric English Comments
Dropping Point 288 °C
550 °F
ASTM D2265
Descriptive Properties Value Comments
Color grey
Soap/Thickener Type calcium sulfonate
Water Spray Resistance, ASTM D4049, % Spray-off 25
Water Washout, ASTM D1264, wt% 1
@ 79°C
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved