Georgia Gulf ProTherm® 4510 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high chemical resistance is required and/or elevated temperatures exist. 4510 has excellent processability, including thermal stability, flow and surface appearance. ProTherm® 4510 listing under NSF Standard 16 and Standard 61 is pending.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D-785
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D-638
Tensile Modulus 2.55 GPa
370 ksi
ASTM D-638
Izod Impact, Notched 0.908 J/cm

@Thickness 6.35 mm
1.70 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 101.0 °C
213.8 °F
annealed; ASTM D-648