Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Rando® HD 46

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Rando® HD 46.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced downtime — Effective rust and oxidation inhibitor system prevents the production of abrasive particles from rust formation, and deposits, varnishes and sludges from oil breakdown, which can damage equipment surfaces and seals, and block filters prematurely.Trouble-free operation — Good hydrolytic stability and water separation characteristics provide excellent filterability in the presence of water contamination. Good anti-foam and air release properties ensure smooth operation and system efficiency.Extended oil service life — High oxidation stability resists oil thickening and deposit formation in service, eliminating the need for unscheduled change of hydraulic fluid.Texaco Rando HD ISO 32, 46, and 68 are designed to give maximum hydraulic pump protection in mobile and stationary systems.Texaco Rando HD ISO 100, 150, and 200 are designed for all types of lubricant applications where a premium antiwear lubricant in their ISO viscosity grade is required, such as an AGMA Gear Lubricant or general machinery lubrication.Texaco Rando HD oils provide excellent:Antiwear protectionOxidation and corrosion inhibitionFoam and aeration suppressionUnder moderate loads and temperatures, the high viscosity index of Texaco Rando HD oils assures good film strength between metal surfaces and is further enhanced by antiwear additive protection.Texaco Rando HD ISO 32, 46, or 68 are recommended for:Vane-, piston-, or gear-type pumps, especially where pressures exceed 1000 psiLightly loaded reciprocating compressorsMotors and bearings.Texaco Rando HD ISO 100, 150, or 220 are recommended for:Hydraulic equipment reduction gearsReciprocating air compressorsPlain and antifriction bearingsCirculating oil systemsTexaco Rando HD oils meet the requirements of:Vickers I-286-S, M-2950-S, 35VQ-25 (ISO 32, 46, 68)Cincinnati Machine P-68 (ISO 32), P-70 (ISO 46), P-69 (ISO 68)Denison HF-0/T6C, HF-2 (ISO 32, 46, 68)ANSI/AGMA 9005-D94, Industrial Gear Lubrication, for gear lubrication as rust and oxidation inhibited gear oils (ISO 46, 68, 100, 150, 220)the U.S. Department of Agriculture (USDA) as H2 lubricants for use in federally inspected meat and poultry plants where no food contact will occur. (ISO 32, 46, 68, 150, 220)Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221658; MSDS Number: 8643
Physical Properties Metric English Comments
API Gravity 31.8 °
31.8 °
Viscosity Measurement 97
97
Viscosity Index
Saybolt Viscosity at 100°F 225 SUS
225 SUS
Saybolt Viscosity at 210°F 48 SUS
48 SUS
Kinematic Viscosity at 40°C (104°F) 43.7 cSt
43.7 cSt
Kinematic Viscosity at 100°C (212°F) 6.5 cSt
6.5 cSt
Oxidative Stability >= 6000 hour
>= 6000 hour
Hours to 2 mg KOH/g acid number; ASTM D943
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
Flash Point 226 °C
439 °F
Descriptive Properties Value Comments
AGMA Grade 1