Axiall 19940 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19940 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
105°C rated insulation compound for 600V, 1/64 wall (18 AWG and larger) and 1000V applications. Approved by UL for THWN-2 (8 AWG and larger) and THW-2 in all sizes and colors. UL approved for 94 HB. UL recognized component for THHN, THW, THWN, TW, THWN-2, THW-2. Oil resistant I and VW-1 rated.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.34 - 1.38 g/cc
1.34 - 1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 97
91 - 97
delayed; ASTM D-2240
Hardness, Shore D 45 - 51
45 - 51
delayed; ASTM D-2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D-638
Elongation at Yield 270.4 %
270.4 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
325 %
325 %
ASTM D-638
100% Modulus 0.0148 GPa
2.15 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D-746
Flammability, UL94 HB
HB
Oxygen Index 28 %
28 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F