Mechanical Properties Metric English Comments
Tensile Stress 8.00 MPa

@Strain 300 %,
Temperature 23.0 °C
1160 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE)
Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer..
Tensile Stress 8.00 MPa

@Strain 2.50 %,
Temperature 120 °C
1160 psi

@Strain 2.50 %,
Temperature 248 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 8.00 MPa

@Strain 5.00 %,
Temperature 150 °C
1160 psi

@Strain 5.00 %,
Temperature 302 °F
Solvay TECHNYL® A 205F PA66, Conditioned
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 8.00 MPa

@Strain 3.11 %,
Time 3.60e+6 sec
1160 psi

@Strain 3.11 %,
Time 1000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.00 MPa

@Strain 2.98 %,
Time 360000 sec
1160 psi

@Strain 2.98 %,
Time 100 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.00 MPa

@Time 3600 sec,
Strain 2.46 %
1160 psi

@Time 1.00 hour,
Strain 2.46 %
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.00 MPa

@Strain 3.22 %,
Time 3.60e+7 sec
1160 psi

@Strain 3.22 %,
Time 10000 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.00 MPa

@Strain 2.76 %,
Time 36000 sec
1160 psi

@Strain 2.76 %,
Time 10.0 hour
isochronous; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 8.00 MPa

@Strain 0.280 %,
Temperature -40.0 °C
1160 psi

@Strain 0.280 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010  (Unverified Data**)
Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers
Tensile Stress 8.00 MPa

@Strain 25.0 %,
Temperature 100 °C
1160 psi

@Strain 25.0 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 8.00 MPa

@Strain 50.0 %
1160 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..
Tensile Stress 8.00 MPa

@Strain 14.96 %,
Temperature 23.0 °C
1160 psi

@Strain 14.96 %,
Temperature 73.4 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 8.00 MPa

@Strain 1.22 %,
Time 360000 sec
1160 psi

@Strain 1.22 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Stress 8.00 MPa

@Strain 1.00 %,
Time 36000 sec
1160 psi

@Strain 1.00 %,
Time 10.0 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST801 BK010A Nylon 66  (Unverified Data**)
Super Toughened Polyamide 66 Information provided by DuPont Performance Polymers
Tensile Stress 8.00 MPa

@Strain 100 %
1160 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G40D-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 8.00 MPa

@Strain 100 %
1160 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 8.00 MPa

@Strain 300 %
>= 1160 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 582A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 8.00 MPa

@Strain 100 %
>= 1160 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 8.00 MPa

@Strain 100 %
1160 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G40D-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G40D-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 8.00 MPa

@Strain 100 %
1160 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly..
Tensile Stress >= 8.00 MPa

@Strain 300 %
>= 1160 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 782A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress 8.00 MPa

@Strain 6.00 %,
Temperature 160 °C
1160 psi

@Strain 6.00 %,
Temperature 320 °F
ISO 527
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
Tensile Stress 8.00 MPa

@Strain 5.00 %,
Time 3.60e+6 sec
1160 psi

@Strain 5.00 %,
Time 1000 hour
100°C; ISO 527
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.