Mechanical Properties Metric English Comments
Tensile Strength 42.0 MPa

@Thickness 0.0500 mm
6090 psi

@Thickness 0.00197 in
ASTM D882-02
NeXolve Clear Optionox® Polyimide Film/Coating
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
Tensile Strength 42.0 MPa
6090 psi
ISO 527
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
GRECO ISOTHANE 2095A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet
Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® 311 Co-Extruded High Impact Fire-Rated Thermoplastic Sheet
Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® 311 MB Co-Extruded High Impact Fire-Rated Thermoplastic Sheet with Microban® Antimicrobial
Features:Color-matched cap, black or off-white substrateThickness ranging from 1.5 mm to 8.9 mmToughness and durabilityEasy to form with good part definitionChemical resistantFire retardantExcellent..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® XD 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses
Features:Tough and durableResistant to cracking and chippingSolid, integral color3500+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualit..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban®
Features:Tough and extremely durableResistant to cracking and chippingSolid, integral color4,000+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantVery low moisture..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® 321 Co-Extruded High Impact Fire Rated Sheet
Features:Metallic cap, black, gray or off-white substrateThickness ranging from 3.18 mm to 8.9 mmTextures: P-3 Velour Matte and P-C Level HaircellImpact resistantEasy to form with good part definiti..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® 331/331d Co-Extruded High Impact Fire Rated Thermoplastic Sheet with Weatherable Acrylic Film Cap
KYDEX® 331 is a co-extruded high impact fire rated thermoplastic sheet with a weatherable cap that offers superior performance for thermoforming. It can also be used as an impact resistant surfa..
Tensile Strength 42.0 MPa
6090 psi
ASTM D638
KYDEX® T MB High Impact Fire Rated Thermoforming Sheet with Microban® Antimicrobial Product
Features:Substitute for FR-ABS sheet with competitive pricing but superior cost/performanceHigher breakage resistanceStandard thicknesses from 0.71 mm to 2.36 mmAmong the most rigid of thermoforming..
Tensile Strength 42.0 MPa
6090 psi
ISO 527-1
Sax Polymers SAXLAC 320 Acrylonitrile Butadiene Styrene
Saxalac 320 is a high impact resistant, easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid..
Tensile Strength 42.0 MPa
6090 psi
ISO 527-1
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene
Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.I..
Tensile Strength 42.0 MPa
6090 psi
ISO 527-1
Sax Polymers SAXLAC 320U Acrylonitrile Butadiene Styrene
Saxalac 320U is an UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH..
Tensile Strength 42.0 MPa
6090 psi
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA
Heat resistance higher than typical PLA is achieved by addition of a nucleating agent and PDLA homopolymer. Increased modulus is produced by addition of talc to the base grade. Data is for samples..
Tensile Strength 42.0 MPa
6090 psi
cond.; DIN 53 455
Hippe PA 11 Nylon 11
Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti..
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Austin Novel Materials Texalan® 290A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Austin Novel Materials Texalan® 490A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Austin Novel Materials Texalan® 495A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Strength 42.0 MPa

@Strain 10.0 %,
Temperature 60.0 °C
6090 psi

@Strain 10.0 %,
Temperature 140 °F
50 mm/min; ISO 527-2
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 42.0 MPa

@Strain 20.0 %,
Temperature 60.0 °C
6090 psi

@Strain 20.0 %,
Temperature 140 °F
50 mm/min; ISO 527-2
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength >= 42.0 MPa
>= 6090 psi
ISO 37
Austin Novel Materials Texalan® 395A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-1695AB Polyester Based TPU
Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd.