Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® TD925H Nylon 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® TD925H Nylon 12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption, with UV and heat stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hrs; ASTM D570
Water Absorption at Saturation 1.4 %
1.4 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 177 °C
351 °F
ASTM D3418