Material Notes:
General purpose reprocessed copolymer, excellent toughness, strength, stiffness and lubricity. Black. Available in UV stabilized grades: R190-B2 (good weatherability); R190-H2B (maximum weatherability).Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.022 cm/cm
0.022 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 8.0 - 10 g/10 min
8.0 - 10 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 18 %
18 %
ASTM D638
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648