Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® P1420 Polycarbonate, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® P1420 Polycarbonate, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1423: with UV stabilizer.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.26 %
0.26 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 107 MPa
15500 psi
ATSM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Modulus 5.80 GPa
841 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ASTM D648
Users viewing this material also viewed the following: