Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 106.9 MPa | 15500 psi | ASTM D638 |
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
PolyOne Edgetek® MLS-195A Polysulfone Alloy - ESD Material
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | |
Cookson Group Plaskon® 3100LS Mineral Filled Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A semiconductor grade encapsulant suitable for a wide range of applications ranging from small SOICs to moderate lead count DIPs... |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | |
MTI ThermoStran® PP-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
Adell AR-13 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
Adell AR-33 Nylon 66, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | 5mm/min; ISO 527 |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ATSM D638 |
Ashley Polymers Ashlene® 527-25G Nylon 66, 25% Glass Reinforced A 25% glass reinforced impact modified Nylon 66.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced A 14% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polyme.. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 461 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 464 Glass Fiber/Bead Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.25% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ATSM D638 |
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general pu.. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
A. Schulman ComAlloy Aqualoy® 150 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ATSM D638 |
Ashley Polymers Ashlene® P1420 Polycarbonate, 20% Glass Reinforced A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1423: with UV stabilizer.Data provided by the manufacturer |