Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 935-40M Nylon 11

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 935-40M Nylon 11.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Moisture Absorption at Equilibrium 1.1 %
1.1 %
65% RH; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ATSM D638
Elongation at Break 290 %
290 %
ASTM D638
Flexural Modulus 0.980 GPa
142 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
0.260 J/cm

@Temperature -40.0 °C
0.487 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 186 °C
367 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Glass Transition Temp, Tg <= -70.0 °C
<= -94.0 °F
ASTM D746
Users viewing this material also viewed the following: