Ashley Polymers Ashlene® 830L Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 830L Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Basic Nylon 6, medium viscosity, lubricated.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 1.6 %
1.6 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH; ASTM D570
Water Absorption at Saturation 9.6 %
9.6 %
ASTM D570
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 83.0 MPa
12000 psi
ATSM D638
Elongation at Break 75 %
75 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Strength 113 MPa
16400 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648