Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 149WO PBT Polyester, 45% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A flame retardant PBT polyester with 45% glass reinforcement, mineral filled.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ASTM D792
Water Absorption 0.075 %
0.075 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.290 J/cm
0.543 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648