Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent processing advantages of unreinforced Nylon 66 while enhancing rigidity, strength, and heat resistance. Vydyne R220/R228 maintains the chemical resistance typical of nylon to a wide variety of chemicals, gasoline, oils, greases, and solvents. Vydyne R220/R228 resins utilize a unique mineral reinforced nylon system developed by Solutia to satisfy the market need for a high-rigidity thermoplastic as an alternative to certain metals. This mineral system provides two key features: (1) isotropic behavior — property development in molded parts is usually independent of flow direction. (2) a reduction in the tendency to develop sink marks in heavy cross sections such as molded-in bosses and ribs. While not sink free, parts made from Vydyne R220/R228 can often permit boss and rib design or wall cross section changes that would not be tolerable in other unreinforced thermoplastic materials. Thus Vydyne R220/R228 resins offer more uniform molded part strength and performance as well as wider latitude in part design. Vydyne R220/R228 are heat stabilized and designed to provide increased ductility and reduced melt viscosity vs. unreinforced materials. This ductility improvement results in tougher, more impact-resistant molded parts. The reduction in melt viscosity enhances overall ease of injection molding, resulting in minor reductions in tensile strength, modulus, and heat distortion temperature. Parts from Vydyne R220/R228 have successfully withstood paint bake oven cycles without significant loss of either dimensional stability or part properties.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ISO 1183
Water Absorption 1.1 %

@Time 86400 sec
1.1 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.6 %
1.6 %
50% RH; ISO 62
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 2.00 mm
0.010 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm

@Thickness 2.00 mm
0.011 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 73.0 MPa
10600 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Elongation at Yield 16 %
16 %
ISO 527
Tensile Modulus 2.60 GPa
377 ksi
ISO 527
Flexural Strength 50.0 MPa
7250 psi
ISO 178
Flexural Modulus 2.30 GPa
334 ksi
ISO 178
Thermal Properties Metric English Comments
Melting Point 258 °C
496 °F
ISO 3146
Processing Properties Metric English Comments
Processing Temperature 280 - 310 °C
536 - 590 °F
Melt Temperature 285 - 305 °C
545 - 581 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Injection Pressure 55.0 - 140 MPa
7980 - 20300 psi
Hold Pressure 55.0 - 140 MPa
7980 - 20300 psi
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Clamp Pressure 29.43 - 68.67 MPa
4268 - 9960 psi
Cushion 0.300 - 0.640 cm
0.118 - 0.252 in
Screw Speed 40 - 120 rpm
40 - 120 rpm