Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 280 °C | 536 °F | |
Nylene® 453 Nylon 6 Dry as molded. Injection molding grade. Nylene 453 is a UV stabilized, high viscosity nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance provided by 453 is a.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-7859 PPO, with carbon fiber, glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour... |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-8541 PPO, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Isotropic shrinkage characteristics.Superheated steam sterilizable.Infor.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa PBT-T30 30% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® NY-4/PL/15/BK Polyamide 612, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 280 °C | 536 °F | maximum surface temperature, curing tube |
Borealis LE0511 Polyethylene Compound, Crosslinkable, Semiconductive LE0511 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0511 is intended for strippable outer semi conductive s.. |
|||
Processing Temperature | 280 °C | 536 °F | maximum surface temperature, curing tube |
Borealis LE0520 Polyethylene Compound, Crosslinkable, Semiconductive LE0520 is a Strippable Semi conductive Insulation Shielding for Power Cables. LE0520 is suitable for use in triple extrusion processes. Strip forces in the range of 3-6 kN/m (7-14 lbs/half inch) ha.. |
|||
Processing Temperature | 280 - 320 °C | 536 - 608 °F | Recommended for injection molding. |
DuPont Selar® PA 3426 Nylon Barrier Resin Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural pro.. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA210GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Heat resistance, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM 15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Processing Temperature | 280 °C | 536 °F | Extrusion, recommended |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based Fields of application: Anti-static masterbatch for olefinicsExamples: Thermoformed and injection molded PP or PE products such as containers and other packaging products. Other applications are film.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-VANCE® AS 838 Anti-static masterbatch, PP based Fields of application: Highly loaded anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Othe.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-VANCE® AS 884 Anti-static masterbatch, PP based Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypr.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp PRIEX® 25093 Maleic Anhydride Grafted PP random copolymer Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, or mineral filled polyp.. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Processing Temperature | 280 - 315 °C | 536 - 599 °F | Injection Temp. |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 280 °C | 536 °F | See Materials Notes |
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Processing Temperature | 280 °C | 536 °F | See Materials Notes |
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-7903 PPO, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-VANCE® AS 4030 Anti-static masterbatch, PP based Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications.. |