Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 1152 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 348 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 446 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 448 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 648 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 752 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® PG 298 Key Features:UnfilledPlatableSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® SAN 31 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® SAN 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 645 PET 45% Glass Reinforced Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 930 PET 30% Glass Reinforced Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car.. |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® Elite HH 1891 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 215 PET - PBT 15% Glass Reinforced Polyester Vypet VNT 215 is a 15% fiberglass reinforced PET/PBT injection molding compound designed for structural applications.Features: High temperature performance; Low warp; High quality surfaceTypical App.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 615 PET 15% Glass Reinforced Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio.. |
|||
Injection Pressure | 55.0 - 85.0 MPa | 7980 - 12300 psi | |
Lavergne VYPET VNT 635A PET 35% Glass Reinforced Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent.. |
|||
Injection Pressure | 55.0 - 140 MPa | 7980 - 20300 psi | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Injection Pressure | 55.0 - 140 MPa | 7980 - 20300 psi | |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Injection Pressure | 55.0 - 140 MPa | 7980 - 20300 psi | |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Injection Pressure | 55.0 - 140 MPa | 7980 - 20300 psi | |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Injection Pressure | 55.0 MPa | 7980 psi | |
Ineos ABS Lustran® 452
(discontinued **) Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoformingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after I.. |
|||
Injection Pressure | 55.0 - 138 MPa | 7980 - 20000 psi | Average value: 84.0 MPa Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |