C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name FILCO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non Ionic Unsaturated Polyester Polymer Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.Applications: Filco 350 has been studied as a primary film forming component of glass fiber sizing for unsaturated polyester matrix strengthening.Consider the following special properties:pseudo-glass consistency of filmgood solubility in vinylic solventsgood compatibility with other typical sizing component formulationsgood compatibility with various unsaturated polyester matrixesgood transparency of reinforced compoundshigh impregnation speed of sized fibers during glass/resin compound preparationIt is recommendable to use Filco 350 in combination with metacrylic radical organosilanes for glass fiber sizing formulation for:roving for translucent sheetsroving for chip/spraychopped strand mat with powder and liquid binder highly soluble in styreneInformation provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Solids Content 44 - 46 %
44 - 46 %
pH 2.0 - 4.0
2.0 - 4.0
Brookfield Viscosity 50 - 250 cP

@Temperature 20.0 °C
50 - 250 cP

@Temperature 68.0 °F
Brookfield RVT spindle 2.2 RPM
Descriptive Properties Value Comments
Appearance Milky Liquid