Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.820 - 0.920 J/g-°C @Temperature 100 - 100 °C |
0.196 - 0.220 BTU/lb-°F @Temperature 212 - 212 °F |
Average value: 0.842 J/g-°C Grade Count:13 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Specific Heat Capacity | 0.820 - 0.900 J/g-°C @Temperature 100 - 100 °C |
0.196 - 0.215 BTU/lb-°F @Temperature 212 - 212 °F |
Average value: 0.837 J/g-°C Grade Count:15 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 20.0 - 100 °C |
0.196 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |
|||
Specific Heat Capacity | 0.820 J/g-°C | 0.196 BTU/lb-°F | ASTM E1269 |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; E1461-01 |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; ASTM E 1952 |
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Specific Heat Capacity | 0.820 J/g-°C | 0.196 BTU/lb-°F | |
Osprey Metals CE13 Al-Si Controlled Expansion Alloy Al-42%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
Silicone Property; Arlon SQA-TMS-052 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |
|||
Specific Heat Capacity | 0.820 J/g-°C @Temperature 100 °C |
0.196 BTU/lb-°F @Temperature 212 °F |
silicone property; Arlon SQA-TMS-052 |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Specific Heat Capacity | 0.821 J/g-°C | 0.196 BTU/lb-°F | |
Mateck Zero Expansion Glass - ZERODUR Optical crystals |