Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 105 µm/m-°C @Temperature 23.0 - 100 °C |
58.3 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data) This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin.. |
|||
CTE, linear | 105 µm/m-°C | 58.3 µin/in-°F | Above Tg |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
CTE, linear | 105 µm/m-°C | 58.3 µin/in-°F | ASTM D696 |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 105 µm/m-°C @Temperature 20.0 - 160 °C |
58.3 µin/in-°F @Temperature 68.0 - 320 °F |
Silicone Property; ASTM E 831 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
CTE, linear | 105 µm/m-°C @Temperature 20.0 - 160 °C |
58.3 µin/in-°F @Temperature 68.0 - 320 °F |
Silicone Property; ASTM E 831 |
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76.. |
|||
CTE, linear | 105 µm/m-°C @Temperature 20.0 - 160 °C |
58.3 µin/in-°F @Temperature 68.0 - 320 °F |
Silicone Property; ASTM E831 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
CTE, linear | 105 µm/m-°C @Temperature 20.0 - 100 °C |
58.3 µin/in-°F @Temperature 68.0 - 212 °F |
|
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
CTE, linear | 105 µm/m-°C @Temperature -30.0 - 80.0 °C |
58.3 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |
|||
CTE, linear | 105 µm/m-°C @Temperature -30.0 - 80.0 °C |
58.3 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E.. |
|||
CTE, linear | 105 µm/m-°C @Temperature -30.0 - 80.0 °C |
58.3 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers DEXPRO® R116 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R116 is a thermoplastic polyolefin elastomeric. It is unfilled, reactor-grade molding compound. Applications: Exterior trim Information provided by Solvay Engineered Polymers.. |
|||
CTE, linear | 105 µm/m-°C @Temperature 20.0 - 160 °C |
58.3 µin/in-°F @Temperature 68.0 - 320 °F |
Silicone Property; ASTM E 831 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |