Polymer Property : Tensile Strength = 685 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon CP-594CX Bulk Compound
Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but ..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate
Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate
Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier
Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber..
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib..