Material Notes:
Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorine compounds, Ethers, Ketones, Esters, Alcohols and HydrocarbonsThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
1.70 g/cc
0.0614 lb/in³
Laminated ETFE Film Property; ASTM D792
Thickness 50.8 microns
2.00 mil
Substrate; Arlon SQA-TMS-003
203 microns
8.00 mil
Side 1; Arlon SQA-TMS-003
254 microns
10.0 mil
Overall thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
67
67
Laminated ETFE Film Property; ASTM D2240
Tensile Strength 8.96 MPa
1300 psi
Silicone Property; ASTM D412
41.4 MPa
6000 psi
Laminated ETFE Film Property; ASTM D638
Elongation at Break 6.0 - 300 %
6.0 - 300 %
Product Property (Plastic Deformation of ETFE Film); ASTM D638
300 %
300 %
Laminated ETFE Film Property; ASTM D638
700 %
700 %
Silicone Property; ASTM D412
Elongation at Yield 0.00 - 6.0 %
0.00 - 6.0 %
Product Property (Elastic Deformation of ETFE Film); ASTM D638
Tear Strength 39.4 kN/m
225 pli
Silicone Property; Arlon SQA-TMS-029
Thermal Properties Metric English Comments
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Laminated ETFE Film Property; Arlon SQA-TMS-022
0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Silicone Property; Arlon SQA-TMS-022
Maximum Service Temperature, Inert 154 °C
310 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 78.7 kV/mm
2000 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Break Strength (ppiw) 13
at 212°F; Arlon SQA-TMS-008
23
at 68°F; Arlon SQA-TMS-008
9
at 302°F; Arlon SQA-TMS-008
Color Translucent
Total Product Weight (oz/yd2) 9.6
Arlon SQA-TMS-025