Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness >= 25.4 microns
>= 1.00 mil
Side 1
>= 102 microns
>= 4.00 mil
Side 2
203 microns
8.00 mil
Prime Coated 1528 Fiberglass, Substrate
279 - 330 microns
11.0 - 13.0 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 40 - 50
40 - 50
Compound Property
Tensile Strength 5.58 - 6.83 MPa
810 - 990 psi
Compound Property
Elongation at Break 450 - 550 %
450 - 550 %
Compound Property
Peel Strength >= 1.05 kN/m
>= 6.00 pli
Bond Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 12 - 14
Uncoated Fabric Break Strength 200 lb/in
Fill Direction, Substrate Property
250 lb/in
Warp Direction, Substrate Property
Copyright © lookpolymers.com All Rights Reserved