Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 515880R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 518581R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 518581R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 30570R020 0.020" (0.508 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Tensile Strength | 5.79 - 6.83 MPa | 840 - 990 psi | Compound Property |
Arlon 51570R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51582R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inform.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51583R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51586R035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51589R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 55596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 30580R030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51344R015 0.015" (0.381 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51344R020 0.020" (0.508 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51420R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 51971R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon R31310R012 Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Aluminized PET FilmSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material .. |
|||
Tensile Strength | 5.58 - 6.83 MPa | 810 - 990 psi | Compound Property |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |