Orbilan ORBILAN® PE 1000 UHMW-PE

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Orbilan
Trade Name ORBILAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Orbilan ORBILAN® PE 1000 UHMW-PE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Orbilan PE 1000 plastics distinguish themselves through their optimal balance of the technical features with regard to wear-resistance and impact resistance. The areas of use range from general machine and plant construction, transport and electroplate techniques, bunker and silo linings to the manufacture of fenders and sluices for hydraulic architecture.Information provided by the manufacturer
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ISO 1183
Molecular Weight >= 5.00e+6 g/mol
>= 5.00e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Ball Indentation Hardness 38.0 MPa
5510 psi
ISO 2039
Tensile Strength, Yield >= 17.0 MPa
>= 2470 psi
ISO 527-1
Elongation at Break >= 350 %
>= 350 %
ISO 527-1
Elongation at Yield <= 15 %
<= 15 %
ISO 527-1
Modulus of Elasticity >= 0.650 GPa
>= 94.3 ksi
ISO 527-1
Charpy Impact, Notched >= 20.0 J/cm²
>= 95.2 ft-lb/in²
ISO 179
Coefficient of Friction 0.14
0.14
DIN 53 375
Thermal Properties Metric English Comments
CTE, linear 150 - 200 µm/m-°C

@Temperature 20.0 - 80.0 °C
83.3 - 111 µin/in-°F

@Temperature 68.0 - 176 °F
DIN 53 752-A
Thermal Conductivity 0.410 W/m-K
2.85 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 80.0 °C
176 °F
continuous
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
continuous
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
DIN 53 482
Descriptive Properties Value Comments
Attrition 100
Sand-Slurry procedure
Water Absorption < 0.01 mg