Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 178 - 330 microns | 7.00 - 13.0 mil | Overall |
Arlon 910-05RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 178 - 330 microns | 7.00 - 13.0 mil | Overall |
Arlon 910-07RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data .. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |