Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
127 microns
5.00 mil
Carrier
1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.467 MPa
1083 psi
Silicone Property; ASTM D412
8.184 MPa
1187 psi
Post Cured Product; ASTM D412
Elongation at Break 711 %
711 %
Silicone Property; ASTM D412
718 %
718 %
Post Cured Product; ASTM D412
Tear Strength 43.5 kN/m
248 pli
Silicone Property; ASTM D624
47.9 kN/m
273 pli
Post Cured Product; ASTM D624
Compression Set 9.0 %
9.0 %
Post Cured Product, Silicone Property; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 25.3 kV/mm
643 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 177 °C
0.500 hour

@Temperature 350 °F
Recommended Cure Cycle
240 min

@Temperature 227 °C
4.00 hour

@Temperature 440 °F
Recommended Postcure Cycle, after 30 minute ramp up cycle
Shelf Life 3.00 Month

@Temperature 21.1 °C
3.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 52
Arlon SQA-TMS-025