Physical Properties Metric English Comments
Thickness 1520 microns
60.0 mil
Parker Chomerics C-Wing™ Heat Spreader
Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. C-Wing spreaders are a cera..
Thickness 1520 microns
59.8 mil
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate
GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Thickness 1520 microns
59.8 mil
Standard; Laminate
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate
GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses
Thickness 1520 microns
59.8 mil
Standard; Laminate
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards..
Thickness 1520 microns
59.8 mil
Standard
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Thickness 1520 microns
60.0 mil
Gauge, nominal
Mid-Mountain Materials ARMATEX® SF45 Silicone Rubber Coated Glass Fabric
Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based...
Thickness 1520 microns
59.8 mil
Standard for Single-Sided Laminate
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced
GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th..
Thickness 1520 microns
60.0 mil
Daikin NEOFLON AF-1500 PFA Film
NEOFLON PFA film is a high performance film made from tetrafluoroethylene and perfluoroalkyl vinyl ether (PFA).Information provided by Daikin Industries.
Thickness 1520 microns
60.0 mil
Daikin NEOFLON NF-1500 FEP Film
NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 30400N060 0.060" (1.52 mm) Uncured Silicone Rubber
Design/Construction: Interleave 1: KodacelProduct: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for ..
Thickness 1520 microns
60.0 mil
Rubber
Arlon 30400R060 0.06" Uncured, Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
Thickness 1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
Thickness 1520 microns
60.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 32980X060 0.060" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material..
Thickness 1520 microns
60.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Thickness 1520 microns
60.0 mil
ASTM D4325
3M Scotch® 31 Heavy Duty Mining Tape
Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of..
Thickness 1520 microns
60.0 mil
Rubber; Arlon SQA-TMS-003
Arlon 30860R060 0.60" Uncured Silicone Rubber on a Kodacel Carrier
Design/Construction:Interleave: 0.003" Low Density PolyethyleneAdd-on: Uncured Silicone RubberSubstrate: Kodacel CarrierThis data represents typical values for the production material and should ..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
Thickness 1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
Thickness 1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. ..
Thickness 1520 microns
60.0 mil
overall; Arlon SQA-TMS-003
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber
Thickness 1520 microns
60.0 mil
Overall
Arlon 55191R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
Thickness 1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,..
Thickness 1520 microns
60.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET
Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use..
Thickness 1520 microns
60.0 mil
Overall; Arlon SQA-TMS-003
Arlon 32400N060 0.060" (1.52 mm) Uncured Silicone Rubber
Design/Construction: Interleave 1: PET carrierSide 1: Uncured Silicone RubberInterleave 2 : PE carrierAppearance: Translucent silicone rubber on polymer linerThis data represents typical values for ..
Thickness 1520 microns
60.0 mil
Side 1; Arlon SQA-TMS-003
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used ..