Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 43.4 kN/m | 248 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 43.4 kN/m | 248 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Soft Clay Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 43.4 kN/m | 248 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 43.5 kN/m | 248 pli | Silicone Property; ASTM D624 |
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Tear Strength | 43.5 kN/m | 248 pli | Silicone Compound; ASTM D624 |
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material.. |
|||
Tear Strength | 43.4 kN/m | 248 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Soft Clay Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 43.4 kN/m | 248 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 60 PHR Non-Black, Mistron Vapor Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 43.4 kN/m | 248 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 40 PHR Dixie Clay Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |