Tensile Strength 7.467 MPa
1083 psi
Silicone Property; ASTM D412
Arlon 32400R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..
Tensile Strength 7.467 MPa
1083 psi
Silicone Property; ASTM D412
Arlon 32400R040 0.040" (1.02 mm) Uncured Silicone Rubber on PET Carrier
Design/Construction:Side 1: Uncured Silicone RubberCarrier: PETInterleave: PolyethyleneAppearance: Red silicone rubber on polymer linerThis data represents typical values for the production material..