Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%

Category Carbon , Graphite
Manufacturer Aremco
Trade Name Pyro-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This carbon and graphite based coating is formulated for parting of aluminum permanent molds, non-sticking in glass forming applications, and lubrication and stop-off in metalworking and wire drawing. Provides superior release, surface finish and mold protection.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
Density 1.14 g/cc
0.0411 lb/in³
Solids Content 29.7 %
29.7 %
volume
45.5 %
45.5 %
weight
pH 8.0 - 9.0
8.0 - 9.0
Coating pH
Viscosity 100 - 250 cP
100 - 250 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2200 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Black
Coverage ft2/gal 475
Theoretical Coverage at 1 mil dry film thickness
Thinner 634-GR-T
Weight/Gallon 9.5 lbs