Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | Upper limit of working range |
Heatbath/Park Carbon Cover C A special blend of graphites suited for cover on neutral salts especially for use with Nu-SalInformation provided by Heatbath Corporation - Park Metallurgical. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast C Sp Dense Refractory Brick Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics CFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics ZAP 010 Smart Cast Application Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | exceptional strength to 1200°C |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | |
Stellar Canada CERAMITE® BKR Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | |
Universal Wire Works X Nickel Alloy Welding Wire Universal Alloy X is a nickel chromium molybdenum alloy that possesses exceptional strength and oxidation resistance up to 2200 degrees F. Alloy X has been found to be highly resistant to stress-cor.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DD Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DM Refractory Sheet TYPE RS-DM Sheet is a moldable form of Type RS-D with a higher density than obtainable from Refractory Sheet Type RS-DA. Type RS-DM is ideally suited for fabricating complex shapes from a flat sheet.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | no load |
Accuratus Accuflect™ Light-Reflecting Ceramic Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics 0.4 Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |