Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95% This carbon and graphite based coating is formulated for parting of aluminum permanent molds, non-sticking in glass forming applications, and lubrication and stop-off in metalworking and wire drawin.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95% This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for se.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 1500 High Temperature Ceramic-Metallic Putty, Ceramic Filled Ceramic-Filled, One-Part, Thixotropic Based Paste.Used Primarily to Seal Boiler Doors and Molten Metal Systems.Easy to Apply and Removable; For uses to 2300°F |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AS1 High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95% This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material. |