Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled
(discontinued **) Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe.. |
|||
Storage Temperature | <= 4.44 °C | <= 40.0 °F | 6 months |
ACC QLE 1050 QSI Quantum Silicones 30 Durometer Clear, Addition Cure, 1-part Elastomer for Coating QLE 1050 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: 100% solids Transparent, ideal for pigmentat.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass |
|||
Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15.. |
|||
Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C). |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C) |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 2400 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Applications to 3/8" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Storage Temperature | 4.44 - 29.4 °C | 40.0 - 85.0 °F | |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95% This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |