Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled
(discontinued **) Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95% This carbon and graphite based coating is formulated for parting of aluminum permanent molds, non-sticking in glass forming applications, and lubrication and stop-off in metalworking and wire drawin.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95% This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for se.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 653 High Temperature Ceramic-Metallic Putty, Stainless Filled Ceramic and Stainless-Filled, One-Part, Water Based Paste.For Vertical Surfaces and Applications to 1/2" Thick.Repairs Cast Iron, Steel and Stainless Parts to 2000°F. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-AS1 High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95% This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo.. |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 1000 High Temperature Ceramic-Metallic Putty, Aluminum Filled Ceramic and Aluminum-Filled, Two-Part, Water Based Paste.For Applications to 1/2" Thick.Repairs Cast Aluminum Parts to 1400°F |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 2500 High Temperature Ceramic-Metallic Putty, Iron Oxide Filled Ceramic and Black Iron Oxide-Filled, One-Part, Water Based Paste.For Applications to 1/4" Thick.Repairs Cast Iron, and Steel Parts to 1600°F |
|||
Storage Temperature | 4.44 - 32.2 °C | 40.0 - 90.0 °F | |
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material. |