| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Aremco |
| Trade Name | Aremco-Seal™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.31 g/cc | 1.31 g/cc | |
| Solids Content | 43.3 % | 43.3 % | by volume |
| 55.8 % | 55.8 % | by weight | |
| Volatile Organic Compounds (VOC) Content | 104.2 g/l | 104.2 g/l | |
| Viscosity | 50.0 - 100 cP | 50.0 - 100 cP | |
| Thickness | 25.4 microns | 1.00 mil | recommended dry film thickness |
| 58.7 microns | 2.31 mil | estimated wet film thickness | |
| Storage Temperature | 12.8 - 29.4 °C | 55.0 - 85.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 482 °C | 900 °F | Continuous |
| Flash Point | >= 100 °C | >= 212 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | <= 29.5 kV/mm | <= 750 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
| Cure Time | >= 6.00 min | >= 0.100 hour | Air Set prior to curing |
| 45.0 min @Temperature 232 °C |
0.750 hour @Temperature 450 °F |
Adequate ventilation is required when curing these products. Outgassing will occur above 300°F and cease after 750°F. An additional 30 minutes is required at the highest service temperature if service temperature is below 750°F. | |
| Shelf Life | 6.00 Month | 6.00 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Translucent-White | |
| Dry Film Coverage ft2/gal | 695 | at 1 mil |
| Thinner | Butyl Cellosolve/Water |