Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 29.5 kV/mm | 750 kV/in | Cured |
Resin Technology Group UV-406 High Clarity, Moisture Resistant, UV Curing Bonder UV 406 is a rapidly curing UV adhesive developed for use in bonding a variety of plastics, glass and metals, where moisture resistance and low shrinkage during cure is critical. Bond strengths on po.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 4570XB025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)< Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass This data represents typical values for the production material. The data should not be .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | |
Saint-Gobain CHR® SG03-03(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® ABS/PBT 1500 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 29.5 kV/mm @Thickness 1.59 mm, Temperature 25.0 °C |
750 kV/in @Thickness 0.0625 in, Temperature 77.0 °F |
|
Cytec EN-9 (Conap) Casting, Potting, and Molding Compound High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 920-10R##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, Red, Rectangular cross-section self-fusing silicone tape. Meets U.S. Military Specification A-A-59163 (supercedes Mil-I-46852C) except for packaging and sampling. The foll.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 920-10T##-P0 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Transparent, Rectangular cross-section, S.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | Arlon SQA-TMS-020 |
Arlon R30711R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | Original; ASTM D4325 |
3M Scotch™ 130C Linerless Rubber Splicing Tape 3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | 24 hrs in water; ASTM D4325 |
3M Scotch™ 130C Linerless Rubber Splicing Tape 3M™ Scotch™ Linerless Rubber Splicing Tape 130C is a high conformable, linerless, ethylene rubber (EPR), high-voltage insulating tape, formulated to provide excellent thermal dissipation of splice.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 32580R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | |
Aclo Accutech Polypropylene HP0315V Homopolymer High Heat Approved to GMP.PP.013 |
|||
Dielectric Strength | >= 29.5 kV/mm | >= 750 kV/in | IPC TM-650 2.5.6.2 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 51100R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Dielectric Strength | <= 29.5 kV/mm | <= 750 kV/in | |
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C) |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | ASTM D149 |
Arlon 44570XB025 0.025" Uncured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not b.. |
|||
Dielectric Strength | >= 29.5 kV/mm | >= 750 kV/in | ASTM D149 |
Arlon 32140R060 0.060" Uncured Silicone Rubber on Release PET Design/Construction:Interleave: 0.0025" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be use.. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 29.5 kV/mm | 750 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |