Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer Toyobo
Trade Name VYLOPET®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.Information provided by Toyobo Co., Ltd
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
0.0090 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D785
Tensile Strength, Ultimate 123 MPa
17800 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Flexural Yield Strength 196 MPa
28400 psi
ASTM D790
Flexural Modulus 9.30 GPa
1350 ksi
ASTM D790
Compressive Yield Strength 108 MPa
15700 psi
ASTM D695
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 36
36
ASTM D1044
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL-746B
Flammability, UL94 V-0

@Thickness 0.907 mm
V-0

@Thickness 0.0357 in
UL-94
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 23.0 kV/mm

@Thickness 2.00 mm
584 kV/in

@Thickness 0.0787 in
ASTM D149
Arc Resistance 85 sec
85 sec
ASTM D495
Comparative Tracking Index 220 V
220 V
IEC test