Material Notes:
STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability and high impact strength.Data provided by Dow Chemical.Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.0 MPa
1890 psi
ASTM Data
Tensile Strength, Yield 14.0 MPa
2030 psi
ASTM Data
Elongation at Break 10 %
10 %
ASTM Data
Tensile Modulus 1.38 GPa
200 ksi
ASTM Data
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
Flammability, UL94 V-0

@Thickness 6.35 mm
V-0

@Thickness 0.250 in
5V; UL94