Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 60 hour
60 hour
Condition B, F50; ASTM D1693
Melt Index of Compound 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
2" per min, Type IV; ASTM D638
Elongation at Break >= 500 %
>= 500 %
2" per min, Type IV; ASTM D638
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746