Material Notes:
40% MR; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ASTM D955
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 5.52 GPa
801 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 119 °C
246 °F
ASTM D648