Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer AlphaGary
Trade Name Evoprene™ COGEE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding or co-extrusion Can be used in food contact applications with the appropriate stabilizer package
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 2781
Viscosity Measurement 26

@Temperature 150 °C
26

@Temperature 302 °F
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ISO 868
Tensile Strength 11.5 MPa
1670 psi
ISO 37
Elongation at Break 520 %
520 %
ISO 37
100% Modulus 0.00270 GPa
0.392 ksi
ISO 37
300% Modulus 0.00540 GPa
0.783 ksi
ISO 37
Adhesive Bond Strength 1.24 MPa
180 psi
abs
Tear Strength 38.0 kN/m
217 pli
ISO 34-B
Compression Set 27 %

@Temperature 23.0 °C,
Time 259000 sec
27 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
75 %

@Temperature 70.0 °C,
Time 79200 sec
75 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
90 %

@Temperature 100 °C,
Time 79200 sec
90 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Ozone Resistance No Cracks
100 pphm / 200 hrs / 20% strain, ISO1431
Users viewing this material also viewed the following: