Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 1050 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 2050 E Industrial Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 440 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Silplusâ„¢ 70 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | IEC 60811-1-1 |
Lucobit Lucofin® 7440 HFFR EBA MDH Cable Sheathing Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 442 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 450 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
Momentive Performance Materials Addisilâ„¢ 452 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | ASTM D412 |
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD .. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | ISO 527 |
Fainplast Compounds Hax™ HF 215 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flame retardancy, improved processabilityInformation provided by Fainplast Compound.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | 300; ISO 37 |
BASF Elastollan SP 806 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
AlphaGary Megolon™ HF 8110 Low Smoke Halogen Free General purpose sheathing compound with good mechanical and processing properties. Application examples include Data Cables, Optical Cables. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
AlphaGary Megolon™ S540E Low Smoke Halogen Free Highly flexible sheathing grade with a low Young's Modulus and excellent fire retardancy, offering improved processability. Application examples include Radio Frequency / Data Optical / Special Fire.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | ISO 37 |
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding.. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | |
AlphaGary Megolon™ S530 Low Smoke Halogen Free Highly flexible sheathing grade with a low Young's Modulus and excellent fire retardancy. Application example includes Radio Frequency. |
|||
Tensile Strength | 11.5 MPa | 1670 psi | ISO 527 |
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound.. |