Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 1.24 MPa | 180 psi | abs |
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding.. |