Polymer Property : Tear Strength = 217 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 38.0 kN/m
217 pli
Type C; ASTM D624
LG Chemical LC670 Polyolefin Elastomer for Polymer Modification
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio..
Tear Strength 38.0 kN/m
217 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2650 ZKS Custom Liquid Silicone Rubber - Automotive
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tear Strength 38.0 kN/m
217 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
Tear Strength 38.0 kN/m
217 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 3286/40 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time..
Tear Strength 38.0 kN/m
217 pli
Shin-Etsu Silicones LIMSâ„¢ KE2090-50AB Elastomer
KE-2090-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Tear Strength 38.0 kN/m
217 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 38.0 kN/m
217 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 38.0 kN/m
217 pli
ISO 34B
Lubrizol Estane® 54643 Polyester-Based Thermoplastic Polyurethane
Feature: Excellent flame retardant properties, matt surface appearance and low surface friction and transparent spherical pelletsUses: Melt roll coated fabrics and calenderingAvailable in Americas, ..
Tear Strength 38.0 kN/m
217 pli
ASTM D624
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
Tear Strength 38.0 kN/m
217 pli
ASTM D624
ELASTO UK Dryflex® 602800S SEBS Based Material, Filled Qualities, 80A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
Tear Strength 38.0 kN/m
217 pli
ASTM D624
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Tear Strength 38.0 kN/m
217 pli
ASTM D624
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Tear Strength 38.0 kN/m
217 pli
notched; ASTM D624 (C)
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA)
Information provided by Arkema Group
Tear Strength 38.0 kN/m
217 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N220 (ISAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 38.0 kN/m
217 pli
ISO 34-B
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer
Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding..
Tear Strength 38.0 - 168 kN/m
217 - 959 pli
Average value: 91.5 kN/m Grade Count:6
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Tear Strength 38.0 kN/m
217 pli
Die B
Momentive Performance Materials FSE7360 Heat Cured Fluorosilicone Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tear Strength 38.0 kN/m
217 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 38.0 kN/m
217 pli
ISO 34-B
AlphaGary Evoprene™ GC 5691 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..